Hot-dip galvanizing is a corrosion-resistant process where steel sheets are immersed in molten zinc and then removed. The finished products are widely used in the manufacturing of components for automobiles, as well as other household appliances and industrial products. Within continuous hot-dip galvanizing lines (CGL), the material selection for the sleeves or bushings of sink rollers (immersed in the zinc bath) and stabilizing rollers (support rollers positioned above the zinc bath) is critical.
Sink rollers are subjected to prolonged immersion in molten zinc or zinc-aluminum alloy baths. Stabilizing rollers are not directly submerged, but they also bear strip tension and indirect thermal radiation. The materials of sleeves or bushings must be suitable for molten zinc and be able to accommodate varying rotational speeds and temperature conditions. Their performance directly impacts production line efficiency, maintenance costs, and coating quality.
Material Selection Sheets Based on Operating Conditions
SYTOP has extensive production experience with components for the hot-dip galvanizing field, spanning many years. We supply production line components to numerous globally renowned enterprises. If you have concerns regarding material selection for bushings and related components, the following precise parameter data compiled from actual operating conditions can serve as a reference to help you choose suitable materials.
| Temperature | Speed (Meter/Minute) | Molten Liquid | Recommended Material | Service Life |
| 680℃-720℃ | >60 MPM | High Al-Si Molten Bath | T 800 | 4-5 days |
| 680℃-720℃ | 40-60 MPM | | T 800 | |
| 480℃-520℃ | 6>60 MPM | ST 4 | 20-25 days | |
| 480℃-520℃ | 40-60 MPM | ST 6 | 20-25 days |
Sink Rollers / Stabilizer Roller Bushings Selection Guidelines
Sink Roller Sleeves
As the core component directly immersed in molten zinc, the sleeve bears maximum loads, strip tension, and severe corrosion—operating under the harshest conditions. The primary dimensions range from Φ150 to 160 mm.
For high-temperature, high-speed applications (680–720°C, >100 MPM) with high-aluminum-silicon molten zinc, we recommend T800 cobalt-based alloy (service life: 4–5 days). For conventional zinc bath conditions at low temperatures and high speeds (480°C–520°C, 60–100 MPM), ST 4 alloy is selected (service life: 20–25 days).
It is better to replace sleeves at the end of the stable period to prevent accelerated wear, which can cause strip vibration and affect coating uniformity.
Stabilizing Roller Bushing
Installed above the zinc pot without direct zinc bath contact, yet subjected to strip tension and indirect thermal radiation, stabilizing roller bushings are critical for strip flatness control.
Material selection prioritizes ST4 / ST6 cobalt-based alloys for balanced moderate wear resistance and thermal corrosion resistance. For low-temperature, low-speed conditions (480°C–520°C, 40–60 MPM), 316 stainless steel serves as an economical alternative.
Its usage cycle aligns with that of the submerged roller bushings, requiring synchronized maintenance planning.
Related Products for Hot-Dip Galvanizing Lines
Scraper
The scraper’s core function is to remove residual zinc dross and impurities from the surface of galvanized steel sheets, ensuring a flat coating finish.
Recommended material: ST 6 cobalt-based alloy. This material offers excellent wear resistance and thermal radiation resistance, withstanding prolonged exposure to high production line temperatures without deformation or excessive wear. It can be supplied as a matched set with core components such as bushings, simplifying procurement and maintenance processes.
Stopper
The stopper primarily seals the ends of bushings to prevent molten zinc or slag from infiltrating the shaft interior and causing component damage. It operates under identical environmental conditions as the bushing.
We recommend selecting the same material as the corresponding bushing (e.g., T800, ST4, ST6) to ensure performance compatibility under identical temperatures and corrosive environments. Secure it via welding or precision assembly to guarantee sealing reliability and extend the overall service life of the shaft system.
Guide Rail
The guide rail provides guidance and positioning during strip steel conveyance, requiring resistance to high-temperature radiation, strip friction, and minor zinc mist corrosion.
Recommended materials: For high-temperature sections (near the zinc pot, temperatures >500°C), use ST6 cobalt-based alloy for excellent high-temperature wear resistance and corrosion resistance. For low-temperature sections (away from the zinc pot, temperatures <500°C), 316L stainless steel offers a higher cost-performance ratio.
The guide rail surface should be polished to reduce the friction coefficient with the strip and minimize the risk of surface scratches.